CAST IRON (GREY IRON - FLAKE GRAPHITE)
-
EN-GJL-150C ( EN 16482 2014)
TASSO Grade EN-GJL-150C (According to EN 16482:2014) This grade offers exceptional machinability and excellent surface finishes, but limited strength and wear resistance. Noise and vibration damping are excellent in this grade.EN-GJL-150C ( EN 16482 2014) Data Sheet / Specifications
Main Elements: Iron, Carbon, Silicon, Manganese, Phosphorous, Sulphur, Others/Alloying
Denstiy: 7,25 gr/cm3 -
EN-GJL- 200C ( EN 16482 2014)
TASSO Grade EN-GJL-200C (According to EN 16482:2014) This grade offers exceptional machinability and excellent surface finishes, but limited strength and wear resistance. Noise and vibration damping are excellent in this grade.EN-GJL- 200C ( EN 16482 2014) Data Sheet / Specifications
Main Elements: Iron, Carbon, Silicon, Manganese, Phosphorous, Sulphur, Others/Alloying
Denstiy: 7,25 gr/cm3 -
EN-GJL- 250C+ ( EN 16482 2014)
TASSO Grade EN-GJL-250 C+ (According to EN 16482:2014) This grade offers a good combination of strength and wear resistance, while still possessing good machinability ad produces excellent surface finishes. Noise and vibration damping are excellent in this grade.EN-GJL- 250C+ ( EN 16482 2014) Data Sheet / Specifications
Main Elements: Iron, Carbon, Silicon, Manganese, Phosphorous, Sulphur, Others/Alloying
Denstiy: 7,25 gr/cm3 -
EN-GJL- 300C ( EN 16482 2014)
TASSO Grade EN-GJL-300C (According to EN 16482:2014) This grade has excellent wear resistance, strength and heat treatment response. It has reasonable machinability and an excellent surface finish. Noise and vibration damping are good in this gradeEN-GJL- 300C ( EN 16482 2014) Data Sheet / Specifications
Main Elements: Iron, Carbon, Silicon, Manganese, Phosphorous, Sulphur, Others/Alloying
Denstiy: 7,25 gr/cm3